Enhancement of electrochemical activity of Ni-rich LiNi0.8Mn0.1Co0.1O2 by precisely controlled Al2O3 nanocoatings via atomic layer deposition

Enhancement of electrochemical activity of Ni-rich LiNi0.8Mn0.1Co0.1O2 by precisely controlled Al2O3 nanocoatings via atomic layer deposition

AUTHOR’S – Ramasamy, H. V., Sinha, S., Park, J., Gong, M., Aravindan, V. et al. (2019).
Journal of Electrochemical Science and Technology, 10(2), 196-205. DOI:10.5229/JECST.2019.10.2.196